Synthesis Gas Conversion over Rh-Mn-WxC/SiO2 Catalysts Prepared by Atomic Layer Deposition

TitleSynthesis Gas Conversion over Rh-Mn-WxC/SiO2 Catalysts Prepared by Atomic Layer Deposition
Publication TypeJournal Article
Year of Publication2018
AuthorsLiu, Y, Zhang, L, Göltl, F, Ball, MR, Hermans, I, Kuech, TF, Mavrikakis, M, Dumesic, JA
JournalACS Catalysis
Volume8
Issue11
Pagination10707-10720
DOI10.1021/acscatal.8b02461