Shape memory effect in nanoindentation of nickel-titanium thin films

TitleShape memory effect in nanoindentation of nickel-titanium thin films
Publication TypeJournal Article
Year of Publication2003
AuthorsShaw, GA, Stone, DS, Johnson, AD, Ellis, AB, Crone, WC
JournalApplied Physics Letters
Volume83
Pagination257-259
Date PublishedJul 14
Accession Number699CT-0018