Enhanced stability of cobalt catalysts by atomic layer deposition for aqueous-phase reactions

TitleEnhanced stability of cobalt catalysts by atomic layer deposition for aqueous-phase reactions
Publication TypeJournal Article
Year of Publication2014
AuthorsLee, JC, Jackson, DHK, Li, T, Winans, RE, Dumesic, JA, Kuech, TF, Huber, GW
JournalEnergy & Environmental Science
Volume7
Pagination1657-1660
Date PublishedMay
DOI10.1039/c4ee00379a