Control of Thickness and Chemical Properties of Atomic Layer Deposition Overcoats for Stabilizing Cu/gamma-Al2O3 Catalysts

TitleControl of Thickness and Chemical Properties of Atomic Layer Deposition Overcoats for Stabilizing Cu/gamma-Al2O3 Catalysts
Publication TypeJournal Article
Year of Publication2014
AuthorsO'Neill, BJ, Sener, C, Jackson, DHK, Kuech, TF, Dumesic, JA
JournalChemsuschem
Volume7
Pagination3247-3251
Date PublishedDec
DOI10.1002/cssc.201402832